Nazwa pierwiastka | Temperatura topnienia [oC] | Temperatura wrzenia [oC] | GΩsto╢µ [g/cm3] |
Ameryk | 994 | 2607 | 11,7 |
Antymon | 630 | 1637 | 6,7 |
Beryl | 1278 | 2970 | 1,848 |
Bor | 2300 | 2550 | 2,34 (krystaliczny) |
Cez | 28,39 | 669,3 | 1,9 |
Chrom | 1857 | 2673 | 7,19 |
Cynk | 419,5 | 907 | 7,13 |
Cyrkon | 1852 | 4370 | 6,5 |
Gal | 29,78 | 2400 | 5,93 |
German | 958,5 | 2830 | 5,323 |
Glin | 660,1 | 2467 | 2,702 |
Hafn | 2150 | 5400 | 13,31 |
Ind | 156,4 | 2010 | 7,28 |
Iryd | 2454 | 4527 | 22,42 |
Kiur | 1350 | ? | 13,5 |
Kobalt | 1495 | 2900 | 8,9 |
Krzem | 1412 | 2355 | 2,33 |
Lit | 180 | 1336 | 0,534 |
Magnez | 650 | 1107 | 1,745 |
Mangan | 1244 | 2097 | 7,43 |
Mied╝ | 1083 | 2595 | 8,93 |
Molibden | 2622 | 4800 | 10,22 |
Nikiel | 1453 | 2732 | 8,9 |
Niob | 2468 | 4927 | 8,58 |
O│≤w | 327,5 | 1744 | 11,34 |
Osm | 3045 | 5027 | 22,48 |
Platyna | 1769 | 4530 | 21,45 |
Pluton | 639,5 | 3327 | 19,81 |
Polon | 254 | 962 | 9,32 |
Potas | 63,6 | 760 | 0,862 |
Proaktyn | 1575 | ? | 15,37 |
Ren | 3180 | 5627 | 21,04 |
RtΩµ | -38,87 | 356,58 | 13,59 |
Rubid | 38,9 | 688 | 1,53 |
Ruten | 2500 | 4100 | 12,2 |
Selen | 217,4 | 684 | 4,81 (metaliczny) |
S≤d | 97,83 | 882,9 | 0,968 |
Srebro | 960,5 | 2140 | 10,49 |
Tal | 303,5 | 1457 | 11,86 |
Tantal | 2996 | 5425 | 16,6 |
Technet | 2140 | 5030 | 11,5 |
Tellur | 449 | 990 | 6,25 |
Tytan | 1668 | 3260 | 4,60 |
Uran | 1132 | 3818 | 18,69 |
Wolfram | 3380 | 5960 | 19,27 |
Z│oto | 1063 | 2966 | 19,29 |
»elazo | 1539 | 3000 | 7,874 |
|